Guides
Supplementary Cementitious Materials and Heat of Hydration
The mix’s heat is not a cooling-crew decision, but it is one of the reasons a mass placement is easy or hard to keep inside a peak limit. Precooling starts the section cooler. The mix decides how much heat then appears.
On this page
The mix lever, described carefully
Supplementary cementitious materials such as fly ash and slag cement are widely used in structural and mass concrete. One reason engineers reach for them, among others such as durability and workability, is that they can change the heat of hydration compared with a mix that relies more heavily on portland cement alone. The details depend on the materials, the replacement, the temperature, and the age at which you care about the heat. Those details are not something we will invent a table for.
If your thermal control plan depends on a particular cementitious combination, that combination has to be in the approved mix. A cooling mobilisation cannot substitute for a mix that was never submitted, and it cannot make a high-heat mix behave like a low-heat one. It can lower the starting temperature of whatever mix you actually place.
We are not mix designers. Nothing on this page is a recommendation to use or avoid a particular material. It is a map of how the mix conversation and the cooling conversation meet.

How the two conversations should meet
On a mass placement, ask what the mix is doing about heat, and what the placement temperature is doing about the starting point. If the mix has already been chosen to moderate heat, precooling may still be required to hit a placement cap or to give the peak a better start. If the mix is a high-early or cement-rich design, precooling may be asked to do more than it reasonably can, and the engineer should be in that conversation before the pour date.
On a hot-weather slab that only has a placement cap, SCM content may hardly enter the cooling discussion at all. Do not import a mass-concrete mix lecture into a job that does not have a peak limit. Do not ignore the mix on a job that does.
See ACI 207, high-early-strength concrete and heat, and placement versus peak.
What we will not do with this subject
We will not quote typical replacement percentages, typical temperature reductions, or brand-name products. We will not take a position in materials shortages or in the debate about a particular ash or slag source. We will read the mix information you are willing to share, insofar as it helps us size a cooling scope, and we will leave the design of the mix with the people who own it.
What to send
If the thermal plan leans on the mix to control heat, include that note and the temperature limits. If the mix is locked and known to be hot, say so. If you cannot share the design, the limits, the section, and the date are still enough to start a cooling conversation, with a wider margin of uncertainty.
If we use slag or fly ash, do we still need cooling?
Maybe. Those materials may moderate heat, but a placement cap or a tight peak can still require precooling. The specification and the mix together decide.
Can you recommend a mix to avoid nitrogen?
No. Mix design stays with your engineer and producer. We will tell you when a simpler cooling method might already be enough.
Does nitrogen change how SCMs hydrate?
Our scope is the temperature of the fresh concrete at injection. Questions about hydration after placement belong to the engineer and the testing plan.
Related Pages
Send Us the Spec and the Pour Date
Tell us the maximum placement temperature, the volume, the location, and when you are pouring.